Källspråk: Engelska
The poultices were allowed to rest on stained surfaces for a 10 min, 20 min, 30 min and 15 hours. A single cleaning application was performed per cleaning regime. In order to mininmize the rate of evaporation and contact with the external atmosphere, wet poultices were covered with a Mylar R film for the duration of the treatment. Following application, paper pulp was removed and the treated surfaces were rinsed by sprying with distilled water.