The poultices were allowed to rest on stained surfaces for a 10 min, 20 min, 30 min and 15 hours. A single cleaning application was performed per cleaning regime. In order to mininmize the rate of evaporation and contact with the external atmosphere, wet poultices were covered with a Mylar R film for the duration of the treatment. Following application, paper pulp was removed and the treated surfaces were rinsed by sprying with distilled water.
अनुबादका लागि चाहिन सक्ने थप जानकारी
kireçtaşı yüzeylerinden pas lekelerini kaldırmanın yolları ile ilgili makalenin bir bölümüdür.

शीर्षक
Lapalar lekeli yüzeyde...
अनुबाद
तुर्केली

moviestrockद्वारा अनुबाद गरिएको
अनुबाद गर्नुपर्ने भाषा: तुर्केली

Lapalar 10 dk, 20 dk, 30 dk ve 15 saat lekeli yüzeyde bırakılmıştır. Temizleme sürecinin her seferinde, tek bir yöntem uygulanmıştır. Buharlaşma oranını azaltmak ve havayla temasını engellemek için lapalar Mylar R filmiyle kaplanmıştır. Sonraki uygulamada hamur alınmış ve tedavi olmuş yüzey arı su sıkılarak temizlenmiştir.
Validated by FIGEN KIRCI - 2009年 अप्रिल 3日 21:06